Chemical Composition:
Element |
% |
Nickel: |
25.0 |
Chromium |
20.0 |
Copper |
1.5 |
Carbon |
0.01 |
Molybdenum |
4.3 |
Indicative Corrosion Data
Chemical |
Resistance |
Alkaline & Salts |
Good |
Hydrochloric Acid |
Not Suitable |
Hydrofluric Acid |
Not Suitable |
Nitric Acid |
Not Suitable |
Organic Acid |
Good |
Phosphoric Acid |
Good |
Seawater |
Good |
Sulfuric Acid |
Not Suitable |
Corrosion rates may vary at different concentrations and temperatures . Each user is advised to carry out their own corrosion test with sample coupon
Material Specification
Alloy/Form |
ASME |
ASTM |
DIN |
Plate, Sheet & Strip |
SA-240 |
A-240 |
17750 |
Rod & Bar |
SA-276 |
A-276 |
17752 |
Forgings |
SA-473 |
A-473 |
- |
Seamless Pipe & Tube |
SA-312 |
A-312 |
17551 |
Welded Pipe |
SA-312 |
A-312 |
- |
Fittings |
SB-366 |
B-366 |
- |
Request For ProposalRequest a Test Coupon
Equipment |
Specification/Rating |
Alloy 904L High Pressure Autoclave |
50 ml-100 litres, Upto 350 bar, 500°C |
Alloy 904L High Pressure Reactors Alloy 904L Hydrogenators |
50 ml -50000 litres, Upto 150 bar, 500°C |
Alloy 904L Continuous Stirred Tank Reactor |
50 ml-100 litres, Upto 350 bar, 500°C |
Alloy 904L Non-Stirred Pressure Vessels |
50 ml-100 litres, Upto 350 bar, 500°C |
Alloy 904L Catalyst Filters for Precious Metals |
As per requirement |
Alloy 904L Magnetic Drive |
As per requirement |
Alloy 904L Mini Magnetic Coupling |
Nano-20, Nano-40, Nano-80 |
All Products, Product Specifications and Data are subject to change.
- Process equipment in chemical industry
- Bleaching equipment in the pulp and paper industry
- Flue gas cleaning
- Desalination
- Seawater handling
- Hydrometallurgy
- Food and beverage
- Pharmaceuticals
- Heat exchangers